Carburized steel component and carburization process
US11624106B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Mar 18, 2020 |
| Grant date | Apr 11, 2023 |
| Priority date | — |
| Expiry date | Jun 30, 2040 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC22C2204/00
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A carburized steel component, comprising a steel base including, by weight percent, from 0.08% to 0.35% carbon, 0.5% to 1.3% manganese, 0% to 0.35% silicon, 0.2% to 2.0% chromium, 0% to 4% nickel, 0% to 0.50% molybdenum, 0% to 0.06% niobium, and a remaining weight percent of iron, and a carburized layer of above 0.35% by weight carbon from a surface of the carburized layer to a carburized layer depth, wherein the carburized layer depth is from 0.5 mm to 3.0 mm, wherein the carburized layer comprises a microstructure including martensite, retained austenite, carbide, and less than 2% by volume non-martensitic transformation products (NMTP), and wherein the carburized layer includes a prior austenite average grain size of 3.0-8.0 microns from the surface to a depth of at least 0.2 mm.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.