Calcination process to produce enhanced ODH catalyst

US11654419B2 · kind B2 · utility

1Cited by
6References
15Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 21, 2021
Grant dateMay 23, 2023
Priority date
Expiry dateJul 10, 2041

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P20/52
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

Mixed metal oxide catalysts having an amorphous content of not less than 40 wt. % are prepared by calcining the catalyst precursor fully or partially enclosed by a porous material having a melting temperature greater than 600° C. in an inert container including heating the catalyst precursor at a rate from 0.5 to 10° C. per minute from room temperature to a temperature from 370° C. to 540° C. under a stream of pre heated gas chosen from steam and inert gas and mixtures thereof at a pressure of greater than or equal to 1 psig having a temperature from 300° C. to 540° C. and holding the catalyst precursor at that temperature for at least 2 hours and cooling the catalyst precursor to room temperature.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.