Activitation of natural pozzolans
US11655186B2 · kind B2 · utility
Assignee
Inventor
Key dates
| Filing date | Jan 8, 2019 |
| Grant date | May 23, 2023 |
| Priority date | — |
| Expiry date | Jan 30, 2042 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02W30/91
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
An activated pozzolan composition includes a fine interground particulate blend of an initially unactivated natural pozzolan and a supplementary cementitious material (SCM) different than the initially unactivated natural pozzolan. The initially unactivated natural pozzolan may include volcanic ash or other natural pozzolanic deposit having a moisture content of at least 3%, and the activated pozzolan composition can have a moisture content less than 0.5% The initially unactivated natural pozzolan may have a particle size less than 1 mm before intergrinding with the SCM. The SCM used to activate the initially unactivated natural pozzolan can be initially coarse or granular with a size greater than 1-3 μm and may include granulated blast furnace slag, steel slag, other metallurgical slag, pumice, limestone, fine aggregate, shale, tuff, trass, geologic material, waste glass, glass shards, basalt, sinters, ceramics, recycled bricks, recycled concrete, refractory materials, other waste industrial products, sand, or natural mineral.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.