Patent · US Active

Method for preparing molecular sieve SCR catalyst, and catalyst prepared therethrough

US11673128B2 · kind B2 · utility

0Cited by
0References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateSep 12, 2019
Grant dateJun 13, 2023
Priority date
Expiry dateNov 20, 2039

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02C20/10
  • WIPO fieldChemical engineering
  • WIPO sectorChemistry

Abstract

A method for preparing a molecular sieve SCR (selective catalytic reduction) catalyst and a prepared catalyst therethrough. In the method, several molecular sieves are mixed and modified by transition metal or rare-earth metal via ion exchange, then loaded Fe by equivalent-volume impregnation, and loaded Cu by one or more liquid ion exchange. This present invention, combined with several techniques, such as modification of stable molecular sieve by transition and rare-earth metal, Fe loading by equivalent-volume impregnation and Cu loading by one or more liquid ion exchange, and after through stable and effective modification and loading control, the obtained catalyst material is coated on a carrier substrate via size mixing and coating process to be prepared into an integral catalyst.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.