Patent · US Active

Method for calibrating internal temperature field of amorphous alloy prepared by spark plasma sintering

US11673192B2 · kind B2 · utility

0Cited by
0References
10Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 6, 2021
Grant dateJun 13, 2023
Priority date
Expiry dateApr 16, 2041

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P10/25
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

The invention belongs to the field of amorphous alloys, and more specifically, relates to a method for calibrating the internal temperature field of amorphous alloy prepared by spark plasma sintering. First, the part required for temperature field calibration inside the bulk amorphous alloy sample obtained by spark plasma sintering is cut into a series of small amorphous alloy samples, and the isothermal crystallization treatment is performed to obtain the crystallization time of different parts of the sample. An annealing-isothermal crystallization experiment is performed on the adopted amorphous alloy powder at different annealing temperatures, and the functional relationship between the annealing temperature and the crystallization time is obtained. The crystallization time of different parts inside the amorphous alloy sample is substituted into this functional relationship, the temperature distribution during the temperature holding stage during the sintering of different parts inside the amorphous alloy sample can be obtained.