Patent · US Active

Diverting agent and method of filling fracture in well using same

US11674073B2 · kind B2 · utility

1Cited by
0References
5Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 9, 2021
Grant dateJun 13, 2023
Priority date
Expiry dateAug 9, 2041

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08L2205/03
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

A diverting agent of the present invention contains a polyvinyl alcohol-based resin, wherein when the diverting agent is added to a 0.48 mass % aqueous solution of guar gum to prepare a mixed solution having a concentration of 12 mass %, a dispersion liquid obtained by dispersing the mixed solution at 30° C. for 60 minutes is pressurized and dehydrated at a pressure of 1 MPa using a pressure dehydration device including a drainage part having a slit having a width of 2 mm, and a regression line represented by an equation (A): y=ax+b (in the equation (A), y is a cumulative dehydration amount (g), x is a square root of a time (minutes) elapsed from start of pressurization, a and b are a slope and an intercept of the regression line, respectively, and 0<x≤2) is calculated by a least squares method from a scatter diagram plotted on a graph in which the square root x of the time is plotted on a horizontal axis and the cumulative dehydration amount y is plotted on a vertical axis, a slope a of the equation (A) satisfies a condition (B): a≤80.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.