Steel reinforcing bar and production method therefor

US11674196B2 · kind B2 · utility

0Cited by
1References
3Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 22, 2018
Grant dateJun 13, 2023
Priority date
Expiry dateJun 9, 2038

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/009
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A steel reinforcing bar contains 0.06 wt % to 0.11 wt % carbon, more than 0 and not more than 0.25 wt % silicon, 0.8 wt % or more and less than 2.0 wt % manganese, more than 0 and not more than 0.01 wt % phosphorus, more than 0 and not more than 0.01 wt % sulfur, 0.01 to 0.03 wt % aluminum, 0.50 to 1.00 wt % nickel, 0.027 to 0.125 wt % molybdenum, more than 0 and not more than 0.25 wt % chromium, more than 0 and not more than 0.28 wt % copper, more than 0 and not more than 0.01 wt % nitrogen, and the remainder being iron and unavoidable impurities. The reinforcing bar has a surface layer and a core. The surface layer has a hardened layer of tempered martensite, and the core has a mixed structure of bainite, ferrite and pearlite.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.