Sintered friction material for railway vehicles and method for producing the same

US11674206B2 · kind B2 · utility

0Cited by
3References
6Claims
0Family size

Assignees

Inventors

Key dates

Filing dateNov 30, 2017
Grant dateJun 13, 2023
Priority date
Expiry dateSep 7, 2038

Classification

  • Technology area (CPC F)Mechanical Engineering; Lighting; Heating
  • CPC primaryF16D2200/0073
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

There is provided a sintered friction material for railway vehicles that has excellent frictional properties and wear resistance even in a high speed range of 280 km/hour or more. The sintered friction material for railway vehicles is a green compact sintered material containing, in mass %, Cu: 50.0 to 75.0%, graphite: 5.0 to 15.0%, one or more selected from the group consisting of magnesia, zircon sand, silica, zirconia, mullite, and silicon nitride: 1.5 to 15.0%, one or more selected from the group consisting of W and Mo: 3.0 to 30.0%, and one or more selected from the group consisting of ferrochromium, ferrotungsten, ferromolybdenum, and stainless steel: 2.0 to 20.0%, with the balance being impurities.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.