Patent · US Active

Anode active material for lithium secondary battery, method of forming the same and lithium secondary battery including the same

US11688854B2 · kind B2 · utility

0Cited by
1References
8Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 11, 2022
Grant dateJun 27, 2023
Priority date
Expiry dateMar 11, 2042

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

An anode active material for a lithium secondary battery and a lithium secondary battery are provided. The anode active material includes a carbon-based particle including pores formed in at least one of an inside of the particle and a surface of the particle and having a pore size of the carbon-based particle is 20 nm or less, and silicon formed at an inside of the pores of the carbon-based particle or on the surface of the carbon-based particle. A peak intensity ratio in a Raman spectrum of silicon defined as I(515)/I(480) is 1.2 or less. Difference between volume expansion ratios of carbon and silicon can be reduced to improve life-span property of the secondary battery.