Case hardening steel
US11702716B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jan 25, 2016 |
| Grant date | Jul 18, 2023 |
| Priority date | — |
| Expiry date | May 4, 2037 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC23C8/22
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A case hardening steel having excellent fatigue resistance is provided at relatively low production cost. A case hardening steel has a chemical composition containing C: 0.10% to 0.30%, Si: 0.10% to 1.20%, Mn: 0.30% to 1.50%, S: 0.010% to 0.030%, Cr: 0.10% to 1.00%, B: 0.0005% to 0.0050%, Sb: 0.005% to 0.020%, and N: 0.0150% or less in a predetermined range, and further containing Al: 0.010%≤Al≤0.120% in the case where B−(10.8/14)N≥0.0003%, and 27/14[N−(14/10.8)B+0.030]≤Al≤0.120% in the case where B−(10.8/14)N<0.0003%.