Nickel oxide sol-gel ink
US11713396B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Dec 29, 2020 |
| Grant date | Aug 1, 2023 |
| Priority date | — |
| Expiry date | Dec 29, 2040 |
Classification
- Technology area (CPC H)Electricity
- CPC primaryH10K85/211
- WIPO fieldBasic materials chemistry
- WIPO sectorChemistry
Abstract
A method for preparing a nickel oxide precursor ink comprising: preparing a solvent comprising diols and alcohol amines; adding nickel nitrate into the solvent to form a nickel nitrate containing solution; adding at least one metal acetate into the nickel nitrate containing solution to form a nickel nitrate and metal acetate containing solution; adding water to the nickel nitrate and metal acetate containing solution to form a nickel oxide precursor mixture; heating the nickel oxide precursor mixture to 60 to 75 Celsius; and cooling the nickel oxide precursor mixture to form the nickel oxide precursor ink.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.