Patent · US Active

Piston with engineered crown coating and method of manufacturing

US11719184B1 · kind B1 · utility

0Cited by
9References
13Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 21, 2022
Grant dateAug 8, 2023
Priority date
Expiry dateJan 21, 2042

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02T10/12
  • WIPO fieldEngines, pumps, turbines
  • WIPO sectorMechanical engineering

Abstract

A steel piston with an engineered coating is provided. A high thermal conductivity material, for example copper, is disposed on first regions of a combustion bowl to reduce hot spots in the piston. A low thermal conductivity material, for example a ceramic, is disposed on second regions of the combustion bowl to reduce loss of heat through the piston. The high thermal conductivity material disposed on the combustion bowl has a surface roughness (Ra) of less than 5 μm to help reflect IR radiation and promote fuel flow. The low thermal conductivity material disposed on the combustion bowl has a surface roughness (Ra) of less than 3 μm to promote fuel flow. The low thermal conductivity material is also disposed on the bowl rim and top ring land, and has a surface roughness (Ra) of greater than 8 μm on the bowl rim and top ring land to retard gas flow.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.