Method for joining metal parts
US11738414B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | May 8, 2020 |
| Grant date | Aug 29, 2023 |
| Priority date | — |
| Expiry date | Aug 22, 2040 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB23K2103/26
- WIPO fieldMachine tools
- WIPO sectorMechanical engineering
Abstract
A method for joining a first metal part with a second metal part, the metal parts having a solidus temperature above 1100° C., includes applying a melting depressant composition on a surface of the first metal part, the melting depressant composition including a melting depressant component that includes at least 25 wt % boron and silicon for decreasing a melting temperature of the first metal part; bringing the second metal part into contact with the melting depressant composition at a contact point on said surface; heating the first and second metal parts to a temperature above 1100° C.; and allowing a melted metal layer of the first metal component to solidify, such that a joint is obtained at the contact point. The boron at least partly originates from a boron compound selected from any of the following compounds: boric acid, borax, titanium diboride and boron nitride. The melting depressant composition and related products are also described.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.