Abstract
An anti-corrosive material contains an ultraviolet curable resin including a polymerizable compound including at least one of a photopolymerizable (meth)acrylate monomer or a photopolymerizable (meth)acrylate oligomer. The anti-corrosive material has a viscosity of 18,900 mPa·s or less. The anti-corrosive material has an elongation rate of 60% or greater as a result of heating at 120° C. for 4,000 hours after curing.