Bendable glass stack assemblies and methods of making the same

US11752730B2 · kind B2 · utility

0Cited by
4References
18Claims
0Family size

Assignee

Inventors

Key dates

Filing dateAug 11, 2015
Grant dateSep 12, 2023
Priority date
Expiry dateMay 8, 2037

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E10/549
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

A stack assembly is provided that includes a glass layer having a thickness, a first and second primary surface and a compressive stress region extending from the second primary surface to a first depth; and a second layer coupled to the second primary surface. The glass layer is characterized by: an absence of failure when the layer is held at a bend radius from about 3 to 20 mm, a puncture resistance of greater than about 1.5 kgf when the second primary surface is supported by (i) an ˜25 μm thick PSA and (ii) an ˜50 μm thick PET layer, and the first primary surface is loaded with a stainless steel pin having a flat bottom with a 200 μm diameter, a pencil hardness of at least 8H, and a neutral axis within the glass layer located between the second primary surface and half of the first thickness.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.