Method for recycling iron and aluminum in nickel-cobalt-manganese solution
US11760655B2 · kind B2 · utility
Assignees
Inventors
Key dates
| Filing date | Aug 3, 2021 |
| Grant date | Sep 19, 2023 |
| Priority date | — |
| Expiry date | Aug 3, 2041 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02W30/84
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
The present invention relates to a method for recycling iron and aluminum in a nickel-cobalt-manganese solution. The method comprises the following steps: leaching a battery powder and removing copper therefrom to obtain a copper-removed solution, and adjusting the pH value in stages to remove iron and aluminum, so as to obtain a goethite slag and an iron-aluminum slag separately; mixing the iron-aluminum slag with an alkali liquor, and heating and stirring same to obtain an aluminum-containing solution and alkaline slag; and heating and stirring the aluminum-containing solution, introducing carbon dioxide thereto and controlling the pH value to obtain aluminum hydroxide and an aluminum-removed solution.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.