Patent · US Active

Method for producing polyacetal fiber

US11761121B2 · kind B2 · utility

0Cited by
5References
9Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 8, 2018
Grant dateSep 19, 2023
Priority date
Expiry dateApr 26, 2040

Classification

  • Technology area (CPC D)Textiles; Paper
  • CPC primaryD02G3/324
  • WIPO fieldTextile and paper machines
  • WIPO sectorMechanical engineering

Abstract

A method for producing a polyacetal fiber that presents an improved whiteness unevenness is provided. According to one embodiment, there is provided a polyacetal fiber production method that yields a polyacetal fiber using an oxymethylene copolymer having a melt index, at 190° C. under a load of 2.16 kg, of 5-60 g/10 min, wherein the production method includes taking off the polyacetal fiber from the discharge nozzle of a spinning apparatus, and drawing the taken-off polyacetal fiber. The tensile elongation E1 of the polyacetal fiber after the taking off is 20%-500%; the tensile elongation E2 of the polyacetal fiber after the drawing is 10%-100%; E1≥E2; and the single fiber thickness of the polyacetal fiber after the drawing is 0.7-5.0 denier.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.