Patent · US Active

Method for preparing lithium borohydride by means of solid-phase ball milling at room temperature

US11807540B2 · kind B2 · utility

0Cited by
1References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 30, 2018
Grant dateNov 7, 2023
Priority date
Expiry dateMay 30, 2040

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/36
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for preparing lithium borohydride by means of room temperature solid phase ball milling, comprising the following steps: uniformly mixing a magnesium-containing reducing agent and a lithium metaborate-containing reducing material under a non-oxidizing atmosphere at room temperature, performing solid phase ball milling, isolating and purifying to obtain lithium borohydride. The method has the advantages of having a simple process, having a controllable and adjustable reaction procedure, having mild reaction conditions, energy consumption being low, costs being low, and output being high, while creating no pollution, being safe and cyclically using boron resources, having important practical significance.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.