Low iron, high redox ratio, and high iron, high redox ratio, soda-lime-silica glasses and methods of making same

US11814315B2 · kind B2 · utility

0Cited by
38References
17Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 30, 2020
Grant dateNov 14, 2023
Priority date
Expiry dateJun 17, 2041

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC03C4/02
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A glass has a basic soda-lime-silica glass portion, and a colorant portion, the colorant portion including total iron as Fe2O3 in the range of at least 0.10 to no more than 2.00 weight percent, a redox ratio in the range of 0.35 to 0.6, and tin metal providing tin in an amount within the range of greater than 0.005 to 5.0 weight percent; the glass product has a tin side and an opposite air side, said tin side of the glass having a higher concentration of tin than the air side, the air side having a uniform concentration of tin from the air side of the glass product towards the tin side of the glass product.