Abstract
To produce a silicon oxide-based negative electrode material containing Li and having uniform distribution of a Li concentration both inside particles and between particles although a C-coating film is formed on a surface, and yet in which generation of SiC is suppressed. A SiO gas and a Li gas are simultaneously generated by heating a Si-lithium silicate-containing raw material under reduced pressure. The Si-lithium silicate-containing raw material includes Si, Li, and O, in which a part of the Si is present as a Si simple substance and the Li is present as lithium silicate. By cooling the generated gases, Li-containing silicon oxide having an average composition of SiLixOy (0.05<x<y and 0.5<y<1.5 are satisfied) is prepared. After adjusting the particle size, a C-coating film having an average film thickness of 0.5 to 10 nm is formed on a surface of particles at a treatment temperature of 900° C. or less.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.