Patent · US Active

High-strength steel allowing low-temperature welding and high-heat input welding and production method thereof

US11821063B2 · kind B2 · utility

0Cited by
0References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 29, 2022
Grant dateNov 21, 2023
Priority date
Expiry dateJul 29, 2042

Classification

  • Technology area (CPC B)Performing Operations; Transporting
  • CPC primaryB23K2103/04
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A high-strength steel allowing low-temperature welding and high-heat input welding and a production method thereof are provided, which belongs to the technical field of steel production. The high-strength steel includes the following chemical components by mass fraction: 0.03-0.16% of C, 0.05-0.5% of Si, 1.0-1.9% of Mn, 0.002-0.02% of P, 0.001-0.01% of S, 0.005-0.07% of Al, 0.005-0.04% of Ti, 0.1-0.5% of Cr, 0.0005-0.005% of B, 0.002-0.01% of Mg+Zr, 0.001-0.008% of O, 0.004-0.01% of N, and the balance of Fe and residual elements. Magnesium and zirconium are added to form magnesium/zirconium oxide, titanium and boron are added to form titanium/boron nitride, and the two types of precipitates work synergistically to improve the microstructure of a heat-affected zone. The method optimizes the chemical composition and production process of existing high-strength steel.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.