Surface-treated steel plate for cell container

US11824212B2 · kind B2 · utility

0Cited by
3References
6Claims
0Family size

Assignee

Inventors

Key dates

Filing dateOct 27, 2021
Grant dateNov 21, 2023
Priority date
Expiry dateOct 27, 2041

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY10T428/27
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

A surface-treated steel sheet for a battery container, including a steel sheet, an iron-nickel diffusion layer formed on the steel sheet, and a nickel layer formed on the iron-nickel diffusion layer (and constituting the outermost layer, wherein when the Fe intensity and the Ni intensity are continuously measured from the surface of the surface-treated steel sheet for a battery container along the depth direction with a high frequency glow discharge optical emission spectrometric analyzer, the thickness of the iron-nickel diffusion layer being the difference between the depth at which the Fe intensity exhibits a first predetermined value and the depth at which the Ni intensity exhibits a second predetermined value is 0.04 to 0.31 μm; and the total amount of the nickel contained in the iron-nickel diffusion layer and the nickel contained in the nickel layer is 4.4 g/m2 or more and less than 10.8 g/m2.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.