Patent · US Active

Process for the preparation of a C20 to C60 wax from the selective thermal decomposition of plastic polyolefin polymer

US11845900B2 · kind B2 · utility

1Cited by
6References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 30, 2017
Grant dateDec 19, 2023
Priority date
Expiry dateMar 30, 2037

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P20/143
  • WIPO fieldBasic materials chemistry
  • WIPO sectorChemistry

Abstract

The present invention relates to a process for the preparation of a C20 to C60 wax from the thermal decomposition of plastic polymer. The present invention provides a vacuum pyrolysis process for preparing a C20 to C60 wax from the thermal decomposition of plastic polyolefin polymer, the method comprising the steps of: i) introducing plastic polyolefin polymer into a thermal reaction zone of a vacuum pyrolysis reactor; ii) heating the plastic polyolefin polymer at sub-atmospheric pressure, wherein the temperature in the thermal reaction zone of the reactor is from 500° C. to 750° C., to induce thermal decomposition of the plastic polyolefin polymer and to form a thermal decomposition product effluent which comprises a major portion by weight of a C20 to C60 wax fraction; and iii) condensing a vapour component of the thermal decomposition product effluent from the vacuum pyrolysis reactor in a multistage condensation comprising a plurality of condensation stages connected in series.