Aluminum alloy with additions of copper, lithium and at least one alkali or rare earth metal, and method of manufacturing the same

US11846010B2 · kind B2 · utility

0Cited by
2References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 21, 2021
Grant dateDec 19, 2023
Priority date
Expiry dateMay 21, 2041

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C21/18
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for making an aluminum alloy includes steps of (1) weighing out starting materials to achieve a mass of material having a composition that includes aluminum, about 1.8 to about 5.6 percent by weight copper, about 0.6 to about 2.6 percent by weight lithium, and at least one of lanthanum up to about 1.5 percent by weight, strontium up to about 1.5 percent by weight, cerium up to about 1.5 percent by weight, and praseodymium up to about 1.5 percent by weight; (2) loading said starting materials into a crucible; (3) inserting said crucible into a chamber; (4) evacuating said chamber to a predetermined vacuum level; (5) melting said starting materials to form a molten mass; and (6) casting said molten mass into a mold.