Method of treating a mining insert
US11898213B2 · kind B2 · utility
Assignees
Inventors
Key dates
| Filing date | Dec 18, 2020 |
| Grant date | Feb 13, 2024 |
| Priority date | — |
| Expiry date | Dec 18, 2040 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB22F2998/10
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method of treating a sintered mining insert including cemented carbide includes the step of subjecting the mining insert to a surface hardening process. The surface hardening process is executed at an elevated temperature of or above 100° C. A mining insert is also provided, wherein the HV1 Vickers hardness measurement increase (HV1%) from the surface region, measured as an average of HV1 measurements taken at 100 μm, 200 μm and 300 μm below the surface, compared to the HV1 Vickers hardness measured in the bulk (HV1bulk), is at least 8.05-0.00350×HV1bulk.