Patent · US Active

Negative electrode including first layer having low compressive strength carbon active material and silicon active material and second layer having high compressive strength carbon active material and nonaqueous electrolyte secondary battery including the same

US11909033B2 · kind B2 · utility

5Cited by
2References
7Claims
0Family size

Assignees

Inventors

Key dates

Filing dateJan 22, 2019
Grant dateFeb 20, 2024
Priority date
Expiry dateJan 27, 2041

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E60/10
  • WIPO fieldElectrical machinery, apparatus, energy
  • WIPO sectorElectrical engineering

Abstract

In a nonaqueous electrolyte secondary battery, a negative electrode mix layer includes a first layer and a second layer disposed successively from a negative electrode collector. The first layer contains a first carbon-based active material having a 10% compressive strength of 3 MPa or less and a silicon-based active material containing Si. The second layer contains a second carbon-based active material having a 10% compressive strength of 5 MPa or more and has a lower content (mass ratio) of the silicon-based active material than the first layer.