Patent · US Active

Method for producing a press-hardened laser welded steel part and press-hardened laser welded steel part

US11911847B2 · kind B2 · utility

0Cited by
1References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateFeb 26, 2019
Grant dateFeb 27, 2024
Priority date
Expiry dateOct 15, 2040

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C38/48
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for producing a part includes providing a first and a second precoated sheet (1,2), butt welding the first and second precoated sheets (1) to obtain a blank (15), and heating the blank (15) to a heat treatment temperature at least 10° C. lower than the full austenitization temperature of the weld joint (22) and at least 15° C. higher than a minimum temperature Tmin: