Method for producing resin sintered body
US11932770B2 · kind B2 · utility
Assignees
Inventors
Key dates
| Filing date | Mar 14, 2022 |
| Grant date | Mar 19, 2024 |
| Priority date | — |
| Expiry date | Mar 14, 2042 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB29K2101/12
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
A method for producing a resin sintered body 1 by applying an ink 3 to thermoplastic resin powder 2 and sintering the powder, the method including the step of immersing an intermediate resin sintered body 1m, which has an unevenly colored region on the surface thereof and the whole of which has been already sintered, in a surface treatment liquid containing sulfuric acid and chromic anhydride, in which the concentration of chromic anhydride is 300 g/L or more, for 5 minutes or longer. When producing a resin sintered body by sintering thermoplastic resin powder, the surface of the resin sintered body can be evenly and sufficiently colored to an extent required without an unevenly colored region on the surface thereof, and also the surface of the resin sintered body can have a good appearance and smoothness.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.