Process for obtaining vanadium oxide from a gasifier slag field
US11945728B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Apr 3, 2019 |
| Grant date | Apr 2, 2024 |
| Priority date | — |
| Expiry date | Jun 24, 2041 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02P10/20
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A process for obtaining vanadium component in the form of vanadium oxide from gasifier slag is disclosed. The process comprises pulverizing the slag to obtain pulverized slag, which is blended with water and an alkali salt to obtain a slurry. The slurry is dried and then roasted in the presence of air to obtain a roasted slag. The roasted slag is leached to obtain a first filtrate comprising the vanadium component. The first filtrate is reacted with a magnesium salt to remove a silica component in the form of a precipitate. The silica free second filtrate is reacted with an ammonium salt to obtain ammonium metavanadate, which is further calcined to obtain the significant amount of vanadium pentoxide (V2O5).
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.