High-strength stainless steel rotor and method for preparing the same

US11951530B2 · kind B2 · utility

0Cited by
0References
14Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 29, 2021
Grant dateApr 9, 2024
Priority date
Expiry dateNov 13, 2041

Classification

  • Technology area (CPC G)Physics
  • CPC primaryG01C19/06
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A high-strength stainless steel rotor and a method for preparing the same, are provided. The high-strength stainless steel rotor, including the following element components by mass percentage: C: 0.03-0.050%, Cr: 14.90-15.80%, Ni: 5.00-5.70%, Cu: 2.20-2.80%, (Nb+Ta): 0.35-0.44%, Mo: 0.45-0.54%, V: 0.06-0.10%, Si: 0.20-0.60%, Mn: 0.40-0.80%, P≤0.010%, S≤0.010%, O≤0.003%, and the balance of iron and inevitable impurities.