Increase in silicon content in the preparation of quartz glass

US11952303B2 · kind B2 · utility

0Cited by
145References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateDec 16, 2016
Grant dateApr 9, 2024
Priority date
Expiry dateApr 1, 2038

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P40/57
  • WIPO fieldMeasurement
  • WIPO sectorInstruments

Abstract

A quartz glass body and a process for the preparation of a quartz glass body is disclosed. One process includes providing a silicon dioxide granulate from a pyrogenic silicon dioxide powder, making a glass melt out of the silicon dioxide granulate and making a quartz glass body out of at least part of the glass melt. In at least one process a silicon component different from silicon dioxide is added. A quartz glass body is obtainable by this process. A light guide, an illuminant and a formed body, are each obtainable by further processing of the quartz glass body.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.