A glass has a coefficient of thermal expansion in a temperature range from 20° C. to 300° C. of 4.5 ppm/K or less, and a T4 temperature, defined as the temperature at which the glass has a viscosity of 104 dPa*s, at 1500° C. or more, and having a reboil propensity score of less than 10 measured in a reboil propensity test. The reboil propensity score is determined as a number of bubbles per glass rod formed from the glass after the reboil propensity test.