Patent · US Active

High-Mn steel and method of producing same

US11959157B2 · kind B2 · utility

0Cited by
2References
3Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJul 31, 2019
Grant dateApr 16, 2024
Priority date
Expiry dateNov 30, 2040

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2211/001
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Provided is a high-Mn steel having excellent low-temperature toughness and excellent surface characteristics. A high-Mn steel comprises: a chemical composition containing, in mass %, C: 0.100 to 0.700%, Si: 0.05 to 1.00%, Mn: 20.0 to 35.0%, P: ≤0.030%, S: ≤0.0070%, Al: 0.010 to 0.070%, Cr: 0.50 to 5.00%, N: 0.0050 to 0.0500%, O: ≤0.0050%, Ti: ≤0.005%, and Nb: ≤0.005%, with a balance consisting of Fe and inevitable impurities; and a microstructure having austenite as a matrix, wherein in the microstructure, a Mn concentration of a Mn-concentrated portion is 38.0% or less, and an average KAM value is 0.3 or more, yield stress is 400 MPa or more, absorbed energy vE−196 in a Charpy impact test at −196° C. is 100 J or more, and percent brittle fracture is less than 10%.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.