Method for manufacturing an environmental barrier
US11976355B2 · kind B2 · utility
0Cited by
4References
12Claims
0Family size
Assignees
Inventors
Key dates
| Filing date | Sep 20, 2021 |
| Grant date | May 7, 2024 |
| Priority date | — |
| Expiry date | Sep 20, 2041 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02T50/60
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
A method for producing a part having improved resistance to oxidation and high temperature-corrosion, includes the formation of an environmental barrier coating on an at least partially ceramic matrix composite material, the environmental barrier coating being formed by direct liquid injection-metal organic chemical vapor deposition.