Method for purifying nickel-cobalt-manganese leaching solution
US11981976B2 · kind B2 · utility
Assignees
Inventors
Key dates
| Filing date | Aug 3, 2021 |
| Grant date | May 14, 2024 |
| Priority date | — |
| Expiry date | Aug 3, 2041 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02W30/84
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
Disclosed is a method for purifying a nickel-cobalt-manganese leaching solution. The method may include: heating a nickel-cobalt-manganese leaching solution, adding a manganese powder thereto, adjusting the pH, reacting same, and filtering same to obtain iron-aluminum slag and a liquid with iron and aluminum removed therefrom; heating the liquid with iron and aluminum removed therefrom, adding a manganese powder thereto, adjusting the pH, reacting same, and filtering same to obtain copper slag and a solution with copper removed therefrom; heating the solution with copper removed therefrom, adding an alkaline solution thereto, adjusting the pH, reacting same, and filtering same to obtain a nickel-cobalt-precipitated solution and nickel-cobalt-manganese hydroxide; and adding water into nickel-cobalt-manganese hydroxide for slurrying, heating same, adding an acidic solution for dissolution, adjusting the pH, reacting same, heating same, adding a manganese powder thereto, adjusting the pH, and filtering same to obtain iron-aluminum slag and a nickel-cobalt-manganese sulfate solution.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.