Patent · US Active

Superalloy seamless tube and preparation method thereof

US12000032B2 · kind B2 · utility

0Cited by
0References
15Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 4, 2020
Grant dateJun 4, 2024
Priority date
Expiry dateFeb 5, 2042

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C30/00
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A superalloy seamless pipe and a preparation method thereof are provided. The superalloy seamless pipe comprises the following components in percentages by weight: C: 0.01-0.06%, Si: 0.40-1.00%, Mn: 0.30-1.00%, P≤0.025%, S≤0.020%, Cr: 15.00-17.00%, Ni: 44.00-46.00%, Al: 2.90-3.90%, Ce: 0.01-0.03%, Ti: 0.10-0.30%, N: 0.03-0.08%, and the balance of Fe and inevitable impurities.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.