Method for preparing portland cement featuring early strength, low shrinkage, and low heat

US12030814B2 · kind B2 · utility

0Cited by
0References
7Claims
0Family size

Assignees

Inventors

Key dates

Filing dateMay 11, 2023
Grant dateJul 9, 2024
Priority date
Expiry dateMay 11, 2043

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02P40/10
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for preparing Portland cement includes: respectively weighing iron slag, copper slag, vanadium slag, and nickel slag and grinding, to yield prefabricated iron slag, prefabricated copper slag, prefabricated vanadium slag, and prefabricated nickel slag; weighing mica and kaolinite, mixing, and grinding to obtain aluminous raw materials; evenly mixing the prefabricated iron slag and the aluminous raw materials, and calcining, to yield an iron-aluminum eutectic mineral; weighing the marble, fluorite, dolomite, and quartz, evenly mixing the marble, fluorite, dolomite, and quartz with the prefabricated copper slag, prefabricated vanadium slag, and prefabricated nickel slag to yield a first mixture; grinding the iron-aluminum eutectic mineral to yield powders, and calcining a second mixture of the first mixture and the powders, to yield the cement clinker; and cooling the cement clinker, and grinding a third mixture of the cooled cement clinker and the gypsum, to yield the Portland cement.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.