Abstract

An austenitic stainless steel material is provided that has excellent sensitization resistance properties even after use for a long time period at an average operation temperature of 400 to 700° C. after welding with higher heat input. The steel material of the present disclosure has a chemical composition which contains, in mass %, C: 0.020% or less, Si: 1.50% or less, Mn: 2.00% or less, P: 0.045% or less, S: 0.0300% or less, Cr: 15.00 to 25.00%, Ni: 9.00 to 20.00%, N: 0.05 to 0.15%, Nb: 0.1 to 0.8%, Mo: 0.10 to 4.50%, and W: 0.01 to 1.00%, and satisfies Formula (1). The content of Nb in a residue obtained by an extraction residue method is, in mass %, 0.050 to 0.267%, and the content of Cr in the residue is, in mass %, 0.125% or less. 21.9Mo+5.9W−5.0≥0  (1).

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.