Window, method of fabricating the same, and display device including the same

US12069828B2 · kind B2 · utility

0Cited by
4References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJun 2, 2020
Grant dateAug 20, 2024
Priority date
Expiry dateNov 28, 2041

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02E10/549
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

A window includes a base layer and a hard coating layer on the base layer. The hard coating layer includes a first layer on the base layer and of a first thickness, and a second layer on the first layer and of a second thickness. The second layer includes an antistatic agent. The hard coating layer has a hardness reduction rate of 50 percent (%) or less expressed as follows.In the equation above, H is a hardness reduction rate (%) of a target layer, D1 is a hardness reduction rate measured from the target layer at a temperature of 60 degrees Celsius (° C.) with a relative humidity of 93%, and D2 is a hardness reduction rate measured from the target layer at a room temperature with a relative humidity of 30%.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.