Artificial graphite, preparation method thereof, secondary battery containing the same and power consuming device
US12074327B2 · kind B2 · utility
0Cited by
0References
16Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Nov 3, 2022 |
| Grant date | Aug 27, 2024 |
| Priority date | — |
| Expiry date | Nov 3, 2042 |
Classification
- Technology area (CPC Y)Emerging Cross-Sectional Technologies
- CPC primaryY02E60/10
- WIPO fieldElectrical machinery, apparatus, energy
- WIPO sectorElectrical engineering
Abstract
An artificial graphite satisfies: PD5t/PD0.5t≤1.35, where PD5t is a compacted density of the artificial graphite measured under a pressure of 5 ton, and PD0.5t is a compacted density of the artificial graphite measured under a pressure of 0.5 ton.