Long glass fiber manufacturing method, and long glass fiber

US12110249B2 · kind B2 · utility

0Cited by
0References
5Claims
0Family size

Assignee

Inventor

Key dates

Filing dateOct 4, 2022
Grant dateOct 8, 2024
Priority date
Expiry dateOct 4, 2042

Classification

  • Technology area (CPC D)Textiles; Paper
  • CPC primaryD01F9/08
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A method for manufacturing glass long fiber using recovered glass fiber, capable of manufacturing glass long fiber in which a recycle rate is increased, increase of a liquid phase temperature of molten glass and narrowing of an operating temperature range of the molten glass are suppressed, and a spinning temperature is low. The method includes a glass melting step of melting a glass raw material containing glass fiber recovered from a glass fiber-reinforced resin molded product, and a glass fiber mineral material to obtain molten glass; and a spinning step of spinning the molten glass to obtain glass long fiber, and a content of the recovered glass fiber in the glass raw material is in the range of 11 to 75% by mass, and differences in the contents of SiO2, Al2O3, B2O3, and CaO between the glass fiber mineral material and the recovered glass fiber satisfy a prescribed relationship.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.