Methods and systems for reducing turbidity of hydraulic fracturing sands
US12115535B1 · kind B1 · utility
1Cited by
5References
20Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Feb 29, 2024 |
| Grant date | Oct 15, 2024 |
| Priority date | — |
| Expiry date | Feb 29, 2044 |
Classification
- Technology area (CPC B)Performing Operations; Transporting
- CPC primaryB65G2201/045
- WIPO fieldChemical engineering
- WIPO sectorChemistry
Abstract
A method for reducing the turbidity of as-mined sand comprising adding water to the as-mined sand to increase its moisture content to between about 5% and about 40% by weight, mixing the sand and water, piling the wet sand on the ground, allowing the sand to rest for a predetermined period of between about 12 hours and about 3 days, then harvesting less than all of the sand from the pile as reduced turbidity sand.