Hot-rolled steel sheet
US12123064B2 · kind B2 · utility
Assignee
Inventors
Key dates
| Filing date | Jan 30, 2020 |
| Grant date | Oct 22, 2024 |
| Priority date | — |
| Expiry date | Oct 19, 2041 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC21D2211/008
- WIPO fieldMaterials, metallurgy
- WIPO sectorChemistry
Abstract
This hot-rolled steel sheet has a predetermined chemical composition, in which a metal microstructure contains, by area %, 3.0% or more of residual austenite, has a ratio L52/L7 of a length L52 of a grain boundary having a crystal orientation difference of 52° to a length L7 of a grain boundary having a crystal orientation difference of 7° about a <110> direction of 0.10 or more and 0.18 or less, has a standard deviation of a Mn concentration of 0.60 mass % or less, and has a tensile strength of 980 MPa or more.
Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.