Patent · US Active

Production method to produce a precision micro-mask including attaching a mask frame to a metal layer by laser welding and an AMOLED display manufactured therefrom

US12127468B2 · kind B2 · utility

0Cited by
2References
10Claims
0Family size

Assignee

Inventor

Key dates

Filing dateDec 5, 2019
Grant dateOct 22, 2024
Priority date
Expiry dateAug 10, 2041

Classification

  • Technology area (CPC H)Electricity
  • CPC primaryH10K71/166
  • WIPO fieldSurface technology, coating
  • WIPO sectorChemistry

Abstract

A production method to fabricate precision micro-mask for the production of ultra-high resolution Active-Matrix Organic Light Emitting Diode (AMOLED) display is disclosed. The production process of the micro-mask includes the following processes: S1, select the substrate and cleaning. S2, fabricate the main body of micro-mask on the substrate. The main body of micro-mask includes sequentially preparation of debonding layer, the first metal layer and the second metal layer; or sequentially preparation of organic polymer layer, the first metal layer and the second metal layer. S3, welding the mask frame to the second metal layer after alignment, fabricate perforation through holes in the main body of the micro-mask based on the requirement of the display subpixel design; or fabricate perforation through holes in the micro-mask based on the requirement of the display subpixel design, then welding the mask frame to the second metal of the main body of the micro-mask. The precision micro-mask is completed after debonding from the substrate. With the precision micro-mask prepared, the high efficiency, ultra-high resolution (>1000 ppi) AMOLED display with Red-Green-Blue, or other color co…