Patent · US Active

Glass fiber-reinforced resin molded article

US12139591B2 · kind B2 · utility

0Cited by
1References
3Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMar 28, 2022
Grant dateNov 12, 2024
Priority date
Expiry dateMar 28, 2042

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC08K2201/004
  • WIPO fieldMacromolecular chemistry, polymers
  • WIPO sectorChemistry

Abstract

In the glass fiber-reinforced resin molded article, the glass fiber has a flat cross-sectional shape having a ratio of the major axis to the minor axis (major axis/minor axis) in the range of 5.0 to 10.0, the thermoplastic resin is polyaryletherketone, the number average fiber length L of the glass fiber having a length of 25 μm or more contained in the glass fiber-reinforced resin molded article is in the range of 50 to 300 μm, the proportion PS of the glass fiber having a length of 25 to 100 μm contained in the glass fiber-reinforced resin molded article is in the range of 20.0 to 60.0%, the proportion PL of the glass fiber having a length of 500 μm or more is in the range of 1.0 to 15.0%; and the L, PS, PL satisfy the following formula (1). 39.5≤L×PS2/(1000×PL)≤82.4  (1)

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.