Patent · US Active

Copper-beryllium alloy with high strength

US12139783B2 · kind B2 · utility

0Cited by
3References
20Claims
0Family size

Assignee

Inventors

Key dates

Filing dateMay 5, 2020
Grant dateNov 12, 2024
Priority date
Expiry dateMay 15, 2040

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC22C9/00
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A process for producing a copper-beryllium alloy product. The process comprises preparing a base alloy having 0.15 wt %-4.0 wt % beryllium and having grains and an initial cross section area. The process further comprises cold working the base alloy to a percentage of cold reduction of area (CRA) greater than 40%, based on the initial cross section area, and heat treating the cold worked alloy to produce the copper-beryllium alloy product. The grain structure of the copper-beryllium alloy product has an orientation angle of less than 45° when viewed along the direction of the cold working. The copper-beryllium alloy product demonstrates a fatigue strength of at least 385 MPa after 106 cycles of testing.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.