Patent · US Active

Process for the recovery of lithium and transition metal using heat

US12152287B2 · kind B2 · utility

0Cited by
2References
11Claims
0Family size

Assignee

Inventors

Key dates

Filing dateApr 1, 2019
Grant dateNov 26, 2024
Priority date
Expiry dateMay 21, 2041

Classification

  • Technology area (CPC Y)Emerging Cross-Sectional Technologies
  • CPC primaryY02W30/84
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

Process for the recovery of transition metal from spent lithium ion batteries containing nickel, wherein said process comprises the steps of (a) heating a lithium containing transition metal oxide material to a temperature in the range of from 400 to 1200° C., (b) treating said heat-treated material with water, (c) treating the solid residue from step (b) with an acid selected from sulfuric acid, hydrochloric acid, nitric acid, methanesulfonic acid, oxalic acid and citric acid, (d) adjusting the pH value to 2.5 to 8, (e) removing compounds of Al, Cu, Fe, Zn or combinations of at least two of the foregoing from the solution or slurry obtained in step (d).

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.