Patent · US Active

Niobium-based alloy strengthened by silicide and turbine having turbine component formed from

US12152293B2 · kind B2 · utility

0Cited by
6References
17Claims
0Family size

Assignee

Inventors

Key dates

Filing dateJan 19, 2023
Grant dateNov 26, 2024
Priority date
Expiry dateJan 19, 2043

Classification

  • Technology area (CPC F)Mechanical Engineering; Lighting; Heating
  • CPC primaryF05D2300/222
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A niobium-silicide based alloy and a turbine having at least a turbine component formed from the niobium-silicide based alloy are provided. The niobium-silicide based alloy comprises: between about 14 atomic percent and about 24 atomic percent titanium (Ti); between about 11 atomic percent and about 19 atomic percent silicon (Si); between about 4 atomic percent and about 8 atomic percent chromium (Cr); between about 2 atomic percent and about 6 atomic percent hafnium (Hf); up to about 4 atomic percent aluminum (Al); between about 0.5 atomic percent and about 1 atomic percent tin (Sn); between about 5 atomic percent and about 15 atomic percent tantalum (Ta); between about 1 atomic percent and about 5 atomic percent tungsten (W); up to about 5 atomic percent rhenium (Re); up to about 5 atomic percent zirconium (Zr); up to about 6 atomic percent yttrium (Y); and a balance of niobium (Nb).