Method of manufacturing Martensitic steel and a Martensitic steel thereof

US12157925B2 · kind B2 · utility

0Cited by
1References
19Claims
0Family size

Assignee

Inventors

Key dates

Filing dateNov 15, 2019
Grant dateDec 3, 2024
Priority date
Expiry dateJun 28, 2041

Classification

  • Technology area (CPC C)Chemistry; Metallurgy
  • CPC primaryC21D2251/04
  • WIPO fieldMaterials, metallurgy
  • WIPO sectorChemistry

Abstract

A martensitic steel including the following elements, expressed in percentage by weight 0.1%≤C≤0.4%; 0.2%≤Mn≤2%; 0.4%≤Si≤2%; 0.2%≤Cr≤1%; 0.01%≤Al≤1%; 0%≤S≤0.09%; 0%≤P≤0.09%; 0%≤N≤0.09%; and can contain one or more of the following optional elements 0%≤Ni≤1%; 0%≤Cu≤1%; 0%≤Mo≤0.1%; 0%≤Nb≤0.1%; 0%≤Ti≤0.1%; 0%≤V≤0.1%; 0.0015%≤B≤0.005%; 0%≤Sn≤0.1%; 0%≤Pb≤0.1%; 0%≤Sb≤0.1%; 0%≤Ca≤0.1%; the remainder composition being composed of iron and unavoidable impurities caused by processing, the microstructure of said steel having microstructure by area percentage including cumulative presence of residual austenite and bainite between 0% and 25%, the remaining microstructure being martensite at least 70%, and with an optional presence of ferrite between 0% and 10%.

Source: USPTO / EPO open patent data. Objective bibliographic and citation counts.