Technique for controlling molecular weight of PHA copolymer produced by halobacterium
US12173347B2 · kind B2 · utility
0Cited by
4References
10Claims
0Family size
Assignee
Inventors
Key dates
| Filing date | Sep 24, 2019 |
| Grant date | Dec 24, 2024 |
| Priority date | — |
| Expiry date | Feb 24, 2042 |
Classification
- Technology area (CPC C)Chemistry; Metallurgy
- CPC primaryC08J2367/04
- WIPO fieldOther special machines
- WIPO sectorMechanical engineering
Abstract
The purpose of the present invention is to provide a PHA, in particular PHBV, having a molecular weight exceeding 3,610,000 and/or a method for producing such a PHA while controlling the molecular weight thereof. Provided is a copolymer of random copolymerization of 3-hydroxybutanoic acid and 3-hydroxyvaleric acid, having a weight-average molecular weight exceeding 3,610,000.